Adamite or Steel Base is a material with Carbon content and mechanical properties between Steel and Iron.The addition of Cr, Ni, Mo and other elements and a special heat treatment process will develop a high wear and fire cracking resistance together with a constant hardness along the working layer.
MATERIAL | GRADE | CHEMISTRY |
BARREL HARDNESS (HSC) |
|||||
C | Si | Mn | Cr | Ni | Mo | |||
Adamite | AD140 | 1.30-1.50 | 0.30-0.60 | 0.70-1.40 | 0.80-1.60 | / | 0.20-0.60 | 38-55 |
AD140 I | 1.30-1.50 | 0.30-0.60 | 0.70-1.10 | 0.80-1.20 | 0.50-1.20 | 0.20-0.60 | 35-50 | |
AD160 | 1.50-1.70 | 0.30-0.60 | 0.70-1.10 | 0.80-1.20 | / | 0.20-0.60 | 40-50 | |
AD160 I | 1.50-1.70 | 0.30-0.60 | 0.80-1.30 | 0.80-2.00 | ≥0.20 | 0.20-0.60 | 40-60 | |
AD180 | 1.70-1.90 | 0.30-0.80 | 0.60-1.10 | 0.80-1.50 | 0.50-2.00 | 0.20-0.60 | 45-60 | |
AD190 | 1.80-2.00 | 0.30-0.80 | 0.60-1.20 | 1.50-3.50 | 1.00-2.00 | 0.20-0.60 | 55-65 | |
AD200 | 1.90-2.10 | 0.30-0.80 | 0.80-1.20 | 0.60-2.00 | 0.60-2.50 | 0.20-0.80 | 50-65 |
TYPICAL PHYSICAL PROPERTIES |
|||
Material | Neck Hardness (HSC) | Tensile Strength (N/mm2) |
Unevenness of Barrel Surface Hardness (HSC) |
AD140 | ≤45 | ≥590 | <5 |
AD140 I | ≤45 | ≥590 | <5 |
AD160 | ≤50 | ≥490 | <5 |
AD160 I | ≤50 | ≥490 | <5 |
AD180 | ≤50 | ≥490 | <5 |
AD190 | ≤50 | ≥490 | <5 |
AD200 | ≤50 | ≥490 | <5 |
Hardness Distribution
Microstructure